166 dtex/288 f+44 dtex涤氨空包纱一步法生产工艺
The Process of 166 dtex/288 f Polyester+44 dtex Spandex Wrapped Yarn by One-Step Method

张国平,沈建峰,费东龙,王海英,费建丰,张小磊
ZHANG Guo-ping,SHEN Jian-feng,FEI Dong-long,WANG Hai-ying,FEI Jian-feng,ZHANG Xiao-lei

摘要(Abstract):

探讨了采用一体机一步法生产多孔166 dtex/288 f+44 dtex涤氨空包纱的主要工艺。结果表明:在一体机上生产时,涤纶的拉伸比选择1.62,上热箱温度控制在185℃,D/Y为1.70,氨纶的牵伸比为3.5,网络喷嘴采用1.6 mm带涡流腔椭圆孔,网络压力控制在0.3 MPa,机台速度为680 m/mim,可使多孔166 dtex/288 f+44 dtex涤氨空包纱生产过程稳定,产品品质可控,性能指标满足客户需求。
The main production process of 166 dtex/288 f polyester + 44 dtex Spandex wrapped yarn by integrated machine and one-step method was discussed. The results show that the production of polyester and Spandesx wrapped yarn is stable, the product quality is controllable and the properties meet customers' needs when the draft ratio of polyester is 1.62, the upper heater temperature is 185 ℃, D/Y is 1.70,the draft ratio of Spandex is 3.5, the elliptical hole with vortex cavity of interlacing jet is 1.6 mm, interlacing pressure is 0.3 MPa, and the machine speed is 680 m/mim.

关键词(KeyWords): 涤氨空包纱;一步法;多孔;生产工艺
polyester and Spandex wrapped yarn;one-step method;porous;production process

Abstract:

Keywords:

基金项目(Foundation):

作者(Author): 张国平,沈建峰,费东龙,王海英,费建丰,张小磊
ZHANG Guo-ping,SHEN Jian-feng,FEI Dong-long,WANG Hai-ying,FEI Jian-feng,ZHANG Xiao-lei

DOI: 10.16090/j.cnki.hcxw.20190703.001

参考文献(References):

扩展功能
本文信息
服务与反馈
本文关键词相关文章
本文作者相关文章
中国知网
分享