热裂解气相色谱-质谱联用法鉴别三种弹性纤维
Identification of Three Elastic Fibers by Pyrolysis Gas Chromatography-Mass Spectrometry

连秋燕,邱尚仁,施点望,裴德君
LIAN Qiu-yan,QIU Shang-ren,SHI Dian-wang,PEI De-jun

摘要(Abstract):

采用热裂解气相色谱-质谱联用技术建立了聚氨酯纤维、二烯类和聚烯烃3种弹性纤维的鉴别方法。裂解温度为600℃时,可以最大限度同时显示聚氨酯纤维、二烯类和聚烯烃3种弹性纤维样品特征。聚氨酯纤维的特征性裂解产物是:不同聚合度(—O—CO—N—)n的中间体;特征离子碎片峰是荷质比(m/z)=71。二烯类纤维的特征性裂解产物是:异戊二烯及它的同分异构体和同系物、柠檬烯及它的同分异构体、β-律草烯及它的同分异构体、西柏烯及它的同分异构体等;特征离子碎片峰是m/z=68、79、93等。聚烯烃纤维的特征性裂解产物是:烯烃和烷烃;特征离子碎片峰是m/z=55、57等。
An identification method of three elastic fibers, polyurethane fiber, elastoliene fiber and polyolefinfiber, were established by pyrolysis gas chromatography-mass spectrometry. As shown by the experimentalresults, it was better to choose 600 ℃ as the pyrolytic temperature in the identification, as more significantcharacteristic information were displayed simultaneously. Polyurethane fiber was identified intermediateproducts of(O—CO—N)_n with varies degree of polymerization. Polyurethane fiber's characteristic frag-ment ion peak was m/z=71. Elastoliene fiber's characteristic pyrolysis products were isoprene and its iso-mers and homologous; Limonene and its isomers; beta-Humulene and its isomers;cembrene and its iso-mers. Elastoliene fiber's characteristic fragment ion peak was m/z=68、79、93 etc. Polyolefin fiber's char-acteristic pyrolysis products were alkene and alkane, characteristic fragment ion peak was m/z=55 and 57 etc.

关键词(KeyWords): 聚氨酯纤维;二烯类纤维;聚烯烃纤维;鉴别;裂解气相色谱-质谱联用
polyurethane fiber;elastoliene fiber;polyolefin fiber;identification;pyrolysis gas chromatography-mass spectrometry

Abstract:

Keywords:

基金项目(Foundation):

作者(Author): 连秋燕,邱尚仁,施点望,裴德君
LIAN Qiu-yan,QIU Shang-ren,SHI Dian-wang,PEI De-jun

DOI: 10.16090/j.cnki.hcxw.2017.06.015

扩展功能
本文信息
服务与反馈
本文关键词相关文章
本文作者相关文章
中国知网
分享