涤纶POY/DTY复合丝生产技术The Technology of Polyester POY and DTY Blended Yarn
杨秀琴,辛长征,王岳安,谢俊霞,尹翠玉
YANG Xiu-qin1,2,XIN Chang-zheng2,WANG Yue-an3,XIE Jun-xia3
摘要(Abstract):
通过对后加工33-H加弹机的设备改造,选择合适的工艺路线,使一股135dtex/72fPOY丝经过加弹后形成DTY,再与另一股86dtex/48fPOY丝网络合股形成涤纶复合丝。生产中,后加工的关键工艺为:未进行假捻变形的POY喂入速度与第二罗拉表面线速度相近,为609m/min,适当降低第二热箱温度在150℃左右,给以适当的网络20个/m,可生产出性能优异的涤纶POY/DTY复合丝。
The modification was made on 33-H draw-texturizing machine and optimum process was used. A DTY which was made from 135 dtex/72 f POY blended with 86 dtex/48 f POY through interlacing to form POY/DTY blended yarn in the modified 33-H DTY machine. The POY processing speed 609 m/min,secondary heater 150 ℃,interlacing degree 20/m were selected in the production.
关键词(KeyWords):
POY;DTY;设备改造;涤纶复合丝
POY,DTY,equipment modification,PET blended yarn